▶ Watch On-Demand | 56 Minutes
On-Demand Session: New Methodologies in Nanoindentation Creep
Learn how new feedback algorithms and elevated-temperature SRJTs improve creep lifetime predictions
Watch Individual Sessions:
Overview on Nanoindentation Creep
High Throughput Assessment of Creep Behavior of Advanced Nuclear Reactor Allows by Nanoindentation
Question and Answer
您需要接受 cookie 才能播放该视频。
Cookie 设置
Introduction; Recorded October 18, 2024
Watch Now | 14 Minutes
Overview on Nanoindentation Creep
您需要接受 cookie 才能播放该视频。
Cookie 设置
Presented by Douglas Stauffer, Ph.D., Senior manager of NI manager, Bruker (October 18, 2024)
PRESENTATION HIGHLIGHTS:
[00:00:00]
Overview of nanoindentation creep
[00:01:02]
Reference frequency testing
[00:02:02]
Nanoindentation creep and strain rate jump comparison
[00:03:20]
Thin films and heterogenous strucutres
[00:04:20]
TI 990 TriboIndenter advanced control methods
[00:06:49]
Advanced control with nanoDMA IV
[00:10:00]
Displacement controlled stress relaxation
Watch Now | 31 Minutes
High Throughput Assessment of Creep Behavior of Advanced Nuclear Reactor Allows by Nanoindentation
您需要接受 cookie 才能播放该视频。
Cookie 设置
Presented by Nathan Mara, Professor, University of Minesota (October 18, 2024)
PRESENTATION HIGHLIGHTS:
[00:00:00]
Introduction and motivations
[00:12:36]
Summary of the SRJT protocol
[00:30:14]
Final remarks
Watch Now | 10 Minutes
Question and Answer
您需要接受 cookie 才能播放该视频。
Cookie 设置
Featured Products and Technology
xSol High Temperature Stage
High temperature, atmosphere controlled characterization
阅读更多
REQUEST MORE INFORMATION
Hysitron TI 990 TriboIndenter
The world's most comprehensive and highest performance nanomechanical test system
阅读更多
REQUEST MORE INFORMATION