▶ Watch On-Demand | 56 Minutes

On-Demand Session: New Methodologies in Nanoindentation Creep

Learn how new feedback algorithms and elevated-temperature SRJTs improve creep lifetime predictions 
Introduction; Recorded October 18, 2024
Watch Now | 14 Minutes

Overview on Nanoindentation Creep

Presented by Douglas Stauffer, Ph.D., Senior manager of NI manager, Bruker (October 18, 2024)

       PRESENTATION HIGHLIGHTS:

  • [00:00:00] Overview of nanoindentation creep
  • [00:01:02] Reference frequency testing
  • [00:02:02] Nanoindentation creep and strain rate jump comparison
  • [00:03:20] Thin films and heterogenous strucutres
  • [00:04:20] TI 990 TriboIndenter advanced control methods
  • [00:06:49] Advanced control with nanoDMA IV
  • [00:10:00] Displacement controlled stress relaxation
Watch Now | 31 Minutes

High Throughput Assessment of Creep Behavior of Advanced Nuclear Reactor Allows by Nanoindentation

Presented by Nathan Mara, Professor, University of Minesota (October 18, 2024)

       PRESENTATION HIGHLIGHTS:

  • [00:00:00] Introduction and motivations
  • [00:12:36] Summary of the SRJT protocol
  • [00:30:14] Final remarks
Watch Now | 10 Minutes

Question and Answer