[00:00:00] During a nanoindentation experiment on metallic materials, what is a good sample preparation process if my sample is very thin (below 1 mm)?
[00:01:23] What are the similarities and differences between PeakForce Q&M and the QI mode (also called Force Volume Mode)?
[00:03:09] For the Q&M technique, is it necessary to calibrate with a sample of known modulus? Or is the Tip calibration sufficient?
[00:06:37] How long would it take to generate an AFM-IR image of a couple of microns in size? And how does that compare to FT-IR?
[00:07:38] Is there a possibility to do some of the AFM measurements in liquids