Dynamic Mechanical Characterization of Polymer Coatings and Thin Films via Nanoindentation
Yusuke Matsuda (DuPont Electronics and Industrial) reviews NanoDMA III with comparisons to macroscale DMA
Presented byYusuke Matsuda, Ph.D., DuPont Electronics and Industrial (March 30, 2022)
PRESENTATION HIGHLIGHTS:
[00:00:00]
Welcome & Introduction
[00:02:00]
The Need for Dynamic Mechanical Properties Characterization at High Temperature
[00:04:04]
Dynamic Nanoindentation at High-Temperature
[00:16:40
] Comparison with Tensile DMA
[00:18:20]
Application #1: Determining Cross-link Density
[00:20:20]
Application #2: Hardness
[00:20:30]
Application #3: Film Development for Semiconductor Fabrication Process
[00:21:26]
Conclusions
[00:22:35]
Q&A with Dr. Matsuda
[00:25:25]
Introduction to Bruker's Newest Metrology Solutions: FilmTek
Featured Products and Technology
Hysitron TI 980 TriboIndenter
Versatile nanomechanical and nanotribological test system for advanced material characterization
詳細はこちら
DOWNLOAD BROCHURE
High-Temperature, High-Throughput Nanoindentation: Quantitative Mechanical Property Mapping and Statistics
(PDF, 1 MB)
xSol High Temperature Stage
High temperature, atmosphere controlled characterization
詳細はこちら
REQUEST MORE INFORMATION
Nanomechanical Test Systems
Stand-alone solutions for highly accurate and reliable quantitative mechanical and tribological characterization at the nano- and microscales
詳細はこちら
RETURN TO SESSION OVERVIEW